In this work, the photodegradation of the carcinogenic pollutant 2-naphthol in aqueous solution containing Aldrich humic acid (HA) and ferric ions (Fe(III)) under 125 W and 250 W high pressure mercury lamp (HPML, lambda >= 365 nm) irradiation was investigated. The photooxidation efficiencies were dependent on the pH values, light intensities and Fe(III)/HA concentration in the water, with higher efficiency at pHs 3-4, and 50 mu mol l(-1) Fe(III) with 20 mg l(-1) HA under 250 W HPML. The initial rate of photooxidation increases with increasing, the initial concentration of 2-naphthol from 10 mu mol l(-1) to 100 mu mol l(-1), while do not change at 50 and 100 mu mol l(-1). However, higher removal efficiency of 2-naphthol is achieved at its lower initial concentration of 10 mu mol l(-1), and initial rate of photooxidation is 0.193 mu mol l(-1) min(-1). Dissolved oxygen (DO) plays an important role in the system containing Fe(III)-HA complexes in which Fenton and photo-Fenton reactions were enhanced in the environment. Hydroxyl radicals produced in HA solution with or without ferric ions were determined by using benzene as free radical scavenger and phenol as scavenging products proportional to hydroxyl radicals. By using UV-Vis and excited fluorescence spectrum techniques, the main photooxidation products, which have higher absorption in the region of 240-340 nm, were found, and the mechanisms for the oxidative degradation is proposed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Photolysis of microcystins by UV irradiation and the effects of different environmental factors on efficiency of UV degradation were studied. The results indicated that the rates of the photolytical degradation reactions of microcystin-LR and RR-follow pseudo-first-order kinetic process. The results also showed that the concentrations of two microcystin variants decreased significantly by UV-C Irradiation; the wavelength and intensitiy of UV irradiation are two very important factors affecting the rate of degradation; temperature and pH value could also affect the half life of degradation rates. When irradiated by weaker UV-Iight, isomerization could be detected in the course of photolytical degradation. The concentrations of two isomers transformed from microcystin-LR reached its maximum at the third minute and decreased with the time afterwards. To simulate photolysis of microcystins in the field water body, microcystins with low concentration were used. It was found that UV-C illumination was capable of decomposing over 95% of microcystins within 40 min. In the presence of humic substances the photodecomposition slowed down to a certain extent. These results are valuable in using UV irradiation for elimination microcystins from raw water.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

(N-4'-methoxy-2-methyl-5-phenyl)-3-pyrryl-ethylidene (isopropylidene) succinic anhydride fulgide, doped in PMMA matrix, exhibits photochromic behavior. The fatigue resistance experiment shows no photodegradation is detected after more than 450 writing-erasing cycles. Study of fulgide material for holographic recording media shows the optimal exposure and the diffraction efficiency is 1047 mJ/cm(2) and 2.26%, respectively, with 10 mum thickness polymer film. Holographic grating with 1680 lines/mm at writing angle theta = 30degrees is also obtained. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this study, conventional TiO2 powder was heated in hydrogen (H-2) gas at a high temperature as pretreatment. The photoactivity of the treated TiO2 samples was evaluated in the photodegradation of sulfosalicylic acid (SSA) in aqueous suspension. The experimental results demonstrated that the photodegradation rates of SSA were significantly enhanced by using the H-2-treated TiO2 catalysts and an optimum temperature for the H-2 treatment was found to be of 500-600 degreesC. The in situ electron paramagnetic resonance (EPR) signal intensity of oxygen vacancies (OV) and trivalent titanium (Ti3+) associated with the photocatalytic activity was studied. The results proved the presence of OV and Ti3+ in the lattice of the H2-treated TiO2 and indicated that both were contributed to the enhancement of photocatalytic activity. Moreover, the experimental results presented that the EPR signal intensity of OV and Ti3+ in the H-2-treated TiO2 samples after 10 months storage was still significant higher than that in the untreated TiO2 catalyst. The experiment also demonstrated that the significant enhancement occurred in the photodegradation of phenol using the H-2-treated TiO2. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Novel 3D wurtzite ZnSe hierarchical nanostructures have been synthesized by a mild hydrothermal treatment. The as-prepared flowerlike nanostructures efficiently catalyze the photodegradation of methylene blue and ethyl violet present in aqueous solutions under UV light irradiation, exhibiting higher photocatalytic activity than the commercially available photocatalysts P25 and ZnSe microspheres. We also demonstrate that flowerlike morphology is important for the excellent photocatalytic activity.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A simple method to prepare titania nanomaterials of core-shell structure, hollow nanospheres and mesoporous nanoparticles has been developed. The core-shell nanostructures with NH4Cl as core and TiO2 center dot xH(2)O-NH4Cl as shell were prepared in nonaqueous system by the deposition on the surface of the aggregated NH4Cl crystals, which could be transformed into mesoporous anatase nanoparticles or hollow nanospheres by calcination at 500A degrees C or extraction with methanol, respectively. The hierarchical mesoporous nanostructures benefited the photocatalytic activities of the resultant titania nanomaterials, demonstrated by the UV light photodegradation of Methyl Orange.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The degradation behavior of polyimide (PMDA-ODA) induced by nitrogen laser irradiation was studied. The changes in the surface morphology and the composition of the irradiated polyimide films were examined by scanning electron microscopy, X-ray photoelectron spectroscopy and FT-IR spectroscopy. The initial reaction was achieved by photochemical degradation of polyimide in the highly electronic excited state by the absorption of a second 337 nm photon. Atmospheric oxygen sequentially reacted with the produced radicals to form a highly oxidized layer. The formation of carbonyl group was enhanced by the heat remaining on the irradiated polyimide film surfaces. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

TiO2 nanoparticle film catalysts with different thicknesses were prepared by plasma-enhanced chemical vapor deposition(PECVD) method and the surfaces were subsequently treated by TiCl4 or O-2 plasma. Two kinds of TiO2 films with different surface properties were obtained. Their surface microstructures and energy levels of surface states were tested by AFM, XRD, SPS, The photocatalytic activities of the catalysts were determined via photodegradation experiments of phenol. The results demonstrated that photocatalytic activities of samples whose surface was treated by O-2 plasma were greater than those treated by TiCl4 plasma. Moreover, photodegradation ratio of phenol during the first hour catalyzed by 0. 17 mu m thickness TiO2 nanoparticle film was greater than other samples. Especially, the difference of photocatalytic activities of TiO2 nanoparticle films treated by TiCl4 or O-2 plasma was respectively explained by energy band theory.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A new approach for the crosslinking of polyimides via the lactamization of spirodilactone unit in polyimide backbone was studied by two means: model reaction and the comparison of the properties of the polyimide precursors to those of the crosslinking polymers. Polyimides 4 and 5 were soluble in N,N'dimethylacetamide (DMAc), dimethylformamide (DMF), dimethylsulfoxide (DMSO), N'-methylpyrrolidone (NMP), and other common organic solvents, whereas their corresponding crosslinking polymers were insoluble in these solvents. The glass transition temperatures for polyimide 5 and its crosslinking polymer were 262 degrees C and 291 degrees C, whereas those for polyimide 4 and its crosslinking polymer were 265 degrees C and 360 degrees C. The weight-loss rate of the crosslinling polymers was apparently slower than that of the precursors when the temperature was >400 degrees C. The 10% weight-loss temperature for the polyimides 4 and 5 was <500 degrees C, whereas that for the crosslinking polymers was close to or above 600 degrees C. The results indicate that this type of crosslinking polymer has good thermal properties. The temperature for the formation of lactam was above 180 degrees C. (C) 1999 John Wiley & Sons, Inc.